MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Reynolds EZ~Spray® Foam Sprayable Rigid Foam
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Product Overview: EZ~Spray® Foam is a polyurethane foam compound that can be conveniently sprayed using Smooth-On’s EZ~Spray® Junior System. Foam cures quickly to strong, lightweight and impact resistant 8 lb. rigid foam that can be used for a variety of applications including making lightweight castings. Foam can also be sprayed over certain rubber mold configurations as a mother mold material. For more information, refer to Smooth-On’s EZ~Spray® Junior manual and video.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.128 g/cc0.128 g/ccASTM D-1475
Viscosity 400 cP400 cPMixed; ASTM D-2393
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min0.167 hourHandling/Tack-Free Time
 10.0 min0.167 hourDemold Time
Pot Life 0.2167 min0.2167 minASTM D-2471
 
Descriptive Properties
Approx. Volumetric Expansion7times
ColorTan
Kgs./Cubic Meter128[kg/m³]
Lbs./Cubic Foot8[lb/ft³]
Mix Ratio1A:1Bby volume
Specific Volume144[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN170 / 296871

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.