SBR 1500 is a general-purpose cold SBR with higher physicals and abrasion resistance than hot polymerized equivalents. It processes readily, provides the highest tensile strength available in cold SBR polymers, and is suitable for products which do not require resistance to staining and discoloration. Unique Features - Cold polymerized styrene-butadiene elastomer
- Highest tensile strength of all cold SBR products
Applications:- Conveyor and power belting
- General mechanical rubber goods
- Tread stocks for heavy-duty service
Information provided by Lion Elastomer |