MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Teknor Apex Uniprene® UN-7100-55 Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Injection Rate: Fast

Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPV
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 555 seconds; ASTM D2240
 60ASTM D2240
 60Change in hardness after 24 hours at 275°F; ASTM D573
Tensile Strength at Break 522.6 psiAcross Flow, Change in tensile strength after 70 hours at 73°F in IRM 903 Oil; ASTM D471
 630 psiFlow; ASTM D412
 649.9 psiIn Air, Across Flow, Change in tensile strength after 24 hours at 275°F; ASTM D573
 670 psiAcross Flow; ASTM D412
Elongation at Break 217.6 %Across Flow, after 70 hours at 73°F in IRM 903 Oil; ASTM D471
 270 %Flow; ASTM D412
 297.6 %In Air, Across Flow, after 24 hours at 275°F; ASTM D573
 320 %Across Flow; ASTM D412
Tear Strength 15.8 kN/mASTM D624
Compression Set 29 %
@Temperature 100 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -76.0 °FASTM D746
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 344 - 416 °F
Middle Barrel Temperature 354 - 426 °F
Front Barrel Temperature 364 - 436 °F
Nozzle Temperature 374 - 446 °F
Zone 1 330 - 400 °F
Zone 2 340 - 410 °F
Zone 3 350 - 420 °F
Zone 5 360 - 430 °F
Die Temperature 374 - 440 °F
Melt Temperature 374 - 446 °FProcessing Temperature
Mold Temperature 95.0 - 140 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceOpaque
Change in Volume (%)0.23After 20 hours at 77°F in IRM 903 Oil

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Uniprene® UN-2533A Thermoplastic Vulcanizate
Teknor Apex Uniprene® 7010-64NT Thermoplastic Vulcanizate
Stellarchem SV-B65E TPV Compound
Shandong Dawn Dawnprene 551N1 TPV (EPDM/PP)
Shandong Dawn Dawnprene 551B1 TPV (EPDM/PP)

PTEKNO906 / 129087

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.