Description: Hostacom™ BR712GC conventional melt flow, 1,300 MPa flexural modulus, UV-stabilized, mineral-filled polypropylene copolymer has an excellent balance of stiffness, impact and weatherability. It was designed primarily for molded-in color automotive interior components. Uses: Automotive interior parts Information provided by Basell. |