MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Teijin Tenax® J HTA40 E15 1K 67tex 15S Poly-acrylonitrile Carbon Fiber
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: HTA40 1K is a high strength/standard modulus, twisted carbon fiber made in Japan for use as a reinforcement in composites for aerospace and other demanding applications. The fiber is produced from poly-acrylonitrile (PAN) precursor and is surface treated to promote adhesion to organic matrix polymers. The epoxy-based sizing material is designed to aid in handling.

Information provided by Teijin Carbon America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.77 g/cc0.0639 lb/in³
Filament Diameter 7.0 µm7.0 µm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 3447 MPa499900 psi
Elongation at Break 1.4 %1.4 %JIS R7601
Tensile Modulus 228 - 248 GPa33100 - 36000 ksiJIS R7601
 
Descriptive Properties
Density68 g/kmLinear density without sizing
Sizing level (%)2.5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ETEIJIN904 / 277914

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.