MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ceradyne Ceralloy® 2710 BeO-SiC  (discontinued **)
Categories: Ceramic; Carbide; Oxide

Material Notes:

Applications:

  • terminations
  • sever wedges
  • load pellets
  • absorbers
  • Features: former industry standard for terminations etc.

    Information provided by Ceradyne Company

    Ceradyne was acquired by 3M in 2012. The product line has been extensively renamed and reconfigured.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 3.02 g/cc
     
    Electrical PropertiesOriginal ValueComments
    Dielectric Constant 23
    @Frequency 1e+10 Hz
     24
    @Frequency 8.00e+9 Hz
     33
    @Frequency 1e+9 Hz
    Dissipation Factor 0.050
    @Frequency 1e+9 Hz
     0.25
    @Frequency 8.00e+9 Hz
     0.25
    @Frequency 1e+10 Hz
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 7.00 µm/m-°C
    @Temperature 20.0 - 1000 °C
    Thermal Conductivity 130 W/m-K
     
    Descriptive Properties
    CompositionBeO+40%SiC

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Yttria Stabilized Zirconia, YSZ
    Boron Carbide, B4C
    CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze
    Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
    MarkeTech Repton 006 Aluminum Oxide

    CCERDN25 / 708

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.