MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Zoltek™ PX30 Carbon Fiber Scrim Fabric
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: ZOLTEK PX30 carbon scrim is a plain leno weave fabric, produced from 100% ZOLTEK OX spun yarns, that undergoes a high temperature, long carbonization soak process to obtain a high purity (99% carbon) mesh material. The resultant chemically inert fabric exhibits superior thermal stability and a low oxidation rate. ZOLTEK PX30 high-purity carbon scrim fabric is a specialized product designed with an open weave construction which is ideal for applications requiring lightweight secondary reinforcement, such as that used in intumescent coating end uses. The scrim fabrics can also be supplied with an FR coated finish to provide easy handling and installation.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 g/cc0.0632 lb/in³
 
Component Elements PropertiesMetricEnglishComments
Carbon, C >= 99 %>= 99 %
 
Descriptive Properties
Areal Weight1.3 oz/yd2. Zoltek PX30 Scrim Fabric.
 1.9 oz/yds typical. Coated Zoltek PX30 Scrim Fabric.
ConstructionPlain leno weave.
Count (w x F)8x4
Standard Width39 inches
Yarn Input2/10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Zoltek™ PX35 Milled Carbon Fiber
Aremco Graphi-Bond™ 551-R
Graphite, Carbon, C
Zoltek™ PX30 SW08 (Satin Weave) Carbon Fiber Fabric
Zoltek™ PX35 UD200 Uni-Directional Carbon Fabric

ECZO848 / 232326

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.