MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil PP1014H1 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Product Description: A homopolymer resin that meets certified requirements for use in Medical and Pharmaceutical applications.

Availability: Europe and North America

Features:

  • Autoclave Sterilizable
  • Ethylene Oxide Sterilizable
  • Low Extractables
  • Steam Sterilizable
Uses:
  • Labware
  • Medical Packaging
  • Medical/Healthcare Applications
Processing Method: Injection Molding

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccExxonMobil Method
Melt Flow 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 71ISO 868
Tensile Strength, Yield 4640 psiISO 527-2/50
Elongation at Yield 7.0 %ISO 527-2/50
Tensile Modulus 203000 psiISO 527-2/1
Flexural Modulus 189000 psiISO 178
Izod Impact, Notched (ISO) 0.950 ft-lb/in²ISO 180/A
Charpy Impact, Notched 1.40 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Crystallization Temperature 237 °CISO 3164
Deflection Temperature at 0.46 MPa (66 psi) 187 °FISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 126 °FISO 75-2/A
Vicat Softening Point 306 °FISO 306/A50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP1013H1 Polypropylene Homopolymer
ExxonMobil PP1074KNE1 Polypropylene Homopolymer
ExxonMobil Exceed™ PP9122 Polypropylene Homopolymer
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications
ExxonMobil PP1024E4 Homopolymer

PEX99396 / 175632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.