MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® L-CD22-M Black Flame Retardant Nylon 12  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Flame Retardant

Material Notes: Description: Graphite filled, medium-viscosity, heat-stabilized

Applications: Dust caps for ignition distributor, parts with improved frictional performance

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Key Words: PA12,MHL,18-030,CD22
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Moisture Absorption at Equilibrium 0.50 %
@Thickness 1.00 mm,
Temperature 23.0 °C
50% R.H.; ISO 62
Water Absorption at Saturation 1.2 %
@Thickness 1.00 mm
ISO 62
Linear Mold Shrinkage 0.0060 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse 0.0090 cm/cm127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPaISO 527-1/2
Tensile Strength, Yield 45.0 MPaISO 527-1/2
Elongation at Break 6.0 %ISO 527-1/2
Elongation at Yield 5.0 %ISO 527-1/2
Tensile Modulus 2.80 GPaISO 527-1/2
Charpy Impact Unnotched 3.40 J/cm²
@Temperature -30.0 °C
ISO 179/1eU
 3.40 J/cm²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.600 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmIEC 60093
Dielectric Constant 5.0
@Frequency 1e+6 Hz
IEC 60250
 7.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 7.00 kV/mmK20/P50; IEC 60243-1
Dissipation Factor 0.033
@Frequency 1e+6 Hz
IEC 60250
 0.058
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 175 VTest Solution A, 100 drops; IEC 60112
 200 VTest Solution A, 50 drops; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
45x15x10 mm; ISO 11359
Melting Point 178 °CPeak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 160 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75
Vicat Softening Point 160 °C50N; ISO 306
 175 °C10N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Descriptive Properties
Electrolytic CorrosionA1 StepIEC 60426

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsamid® AESN BLACK P202 T6L PA12-I
RTP Company RTP 299 F X 125585 H Nylon 12 (PA); Flame Retardant - Halogen Free
EMS-Grivory Grilamid® L 20H FWA black 9225 PA12
EMS-Grivory Grilamid® L 20 HL black 9563 PA12
Evonik Vestamid® X7167 Flame Retardant Nylon 12

PHULA41 / 47401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.