MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polykemi AB POLYfill PPH TS15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes:

Information provided by Polykemi AB

Key Words: Polypropylene Homopolymer
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Filler Content 10 %10 %±2%; Polykemi
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm0.013 - 0.016 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.013 - 0.016 cm/cm0.013 - 0.016 in/inISO 2577
Melt Index of Compound 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break <= 32.0 MPa<= 4640 psiISO/R527
Elongation at Yield 8.0 %8.0 %ISO/R527
Flexural Strength <= 42.0 MPa<= 6090 psiISO 178
Flexural Modulus 1.70 GPa
@Temperature 23.0 °C
247 ksi
@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C219 °F120°C/h; ISO 75/1
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °F120°C/h; ISO 75/1
Vicat Softening Point  82.0 °C
@Load 5.001 kg
180 °F
@Load 11.03 lb
50°C/h; ISO 306
 144 °C
@Load 1.00 kg
291 °F
@Load 2.21 lb
50°C/h; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 205 - 260 °C401 - 500 °F
Mold Temperature 40.0 - 80.0 °C104 - 176 °F
Drying Temperature 70.0 - 80.0 °C158 - 176 °F
Dry Time 2 - 4 hour2 - 4 hourin circulation dryer
 2 - 4 hour2 - 4 hourin desiccant air dryer
Injection Pressure 40.0 - 110 MPa5800 - 16000 psi
Back Pressure 1.00 - 2.00 MPa145 - 290 psi
 
Descriptive Properties
Holding Pressure20-40% of injection pressure
Injection SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sax Polymers SAXALEN PPH335T20 Polypropylene Homopolymer, 20% Talc Filled
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled
BASF Procom® T20H S63 Polypropylene
BASF Procom® T20C 556 Polypropylene
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled

PPOLYK401 / 123126

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.