High purity stearate with low soluble salt level that reduces discoloration during processing. STRUKTOL® Aluminum Stearate is used by the rubber and plastic industries as an effective elastomer processing aid and release agent. It is an excellent dusting agent to prevent surface adhesion in ABS plastic and in other thermoplastics with minimal discoloration. FDA Status: 173.340; 175.105; 175.210; 175.300; 175.320; 176.170; 176.200; 177.1200; 177.2260; 177.2800 |