MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Network Polymers Softflex® 7210 Black
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: Description: Softflex® Thermoplastic Elastomer Alloy

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm
@Thickness 3.17 mm
0.016 - 0.018 in/in
@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
@Thickness 3.17 mm
0.014 - 0.016 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow  3.1 g/10 min
@Load 1.00 kg,
Temperature 235 °C
3.1 g/10 min
@Load 2.20 lb,
Temperature 455 °F
Procedure A Condition Q; ASTM D1238
 19.7 g/10 min
@Load 2.16 kg,
Temperature 230 °C
19.7 g/10 min
@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
 28.6 g/10 min
@Load 5.00 kg,
Temperature 200 °C
28.6 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 67 - 7767 - 77Instantaneous; ASTM D2240
Tensile Strength, Yield 9.65 MPa1400 psichs 20 in/min; ASTM D412
Elongation at Break 800 %800 %ASTM D412
Tear Strength 43.8 kN/m250 pli

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4340 Steel, annealed, 25 mm round
Assab Steels PRODAX Aluminum Alloy for Plastic Molds
AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
Bohler-Uddeholm P20 PREMIUM MODIFIED Pre-hardened Mold Steel
Bohler-Uddeholm IMPAX® P20 Hot Work Tool Steel

PDIAM021 / 29859

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.