MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Schott LG-940 Phosphate Laser Glass
Categories: Ceramic; Glass; Optical

Material Notes: The LG-940 is an Erbium – Ytterbium – Chromium – Cerium doped phosphate based laser glass used in flash lamp pumped and diode pumped solid-state laser systems. Phosphate glasses generally offer higher solubility of rare earth dopants, thus the amount of active ions can be significantly increased.

Applications

  • Medical lasers for dermatological use
  • Analytical instrumentation
  • Rangefinders
Advantages
  • Good athermal properties
  • High transmission at the lasing wavelength
  • Consistent quality and high homogeneity

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.04 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Class, SR 4.3pH = 0.3 at 25 °C
Alkali Class, AR 3.3pH = 12 at 50 °C
Stain Resistance Class, FR 0.00pH = 4.6 100 h at 25 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Knoop 3800.1/20
Modulus of Elasticity 57.6 GPa
Poissons Ratio 0.26
Shear Modulus 22.9 GPaCalculated
 
Thermal PropertiesOriginal ValueComments
CTE, linear 81.1 µm/m-°C
@Temperature 20.0 - 40.0 °C
 119.6 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 0.510 W/m-K
@Temperature 25.0 °C
 0.610 W/m-K
@Temperature 90.0 °C
Transformation Temperature, Tg 456 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.533
 1.522
@Wavelength 1540 nm
Transmission, Visible 62.2 %
 
Descriptive Properties
Climatic resistance1-2Water Vapor at 40 – 50 °C for 30 h

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CSGT9941 / 183194

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.