MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type 302B Stainless Steel, annealed plate
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Austenitic Cr-Ni stainless steel. More corrosion resistant than Type 301 and because of higher Ni content does not work harden as quickly as Type 301. Essentially non-magnetic in annealed condition, slightly magnetic in cold worked condition. Can be stamped, blanked, formed, and lightly drawn. Applications include car and radar antennas, automobile trim, bottling machinery, dairy processing equipment, food processing equipment, home appliances, hospital equipment, industrial floor plate, jewelry, kitchen and restaurant equipment, spring clips, washers, retainers.

Key Words: T302, T 302, 302SS, 302 SS, UNS S30215, ASTM A167, ASTM A276, ASTM A314, ASTM A473, ASTM A580, SAE J405 (30302B), DIN 1.4330, austenitic, 18-8
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 147Converted from Rockwell B hardness.
Hardness, Knoop 164Converted from Rockwell B hardness.
Hardness, Rockwell B 85
Hardness, Vickers 169Converted from Rockwell B hardness.
Tensile Strength, Ultimate 620 MPa
Tensile Strength, Yield 275 MPa
@Strain 0.2 %
Elongation at Break 50 %in 50 mm
Tensile Modulus 195 GPa
Izod Impact 108 Jwhen annealed
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000720 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.008at RT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 0.000 - 100 °C
 18.0 µm/m-°C
@Temperature 0.000 - 315 °C
 19.4 µm/m-°C
@Temperature 0.000 - 540 °C
 20.2 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 15.9 W/m-K
@Temperature 0.000 - 100 °C
 21.6 W/m-K
@Temperature 500 °C
Melting Point 1370 - 1400 °C
Solidus 1370 °C
Liquidus 1400 °C
Maximum Service Temperature, Air 870 °CIntermittent
 925 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 18 %
Iron, Fe 68 %
Manganese, Mn <= 2.0 %
Nickel, Ni 9.0 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 3.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
304 Stainless Steel
301 Stainless Steel
AISI Type 302B Stainless Steel, annealed bar
302 Stainless Steel, annealed strip
302 Stainless Steel, annealed bar

MQ302BH / 12654

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.