MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Imerys Minspar™ 4 Ground Feldspar
Categories: Ceramic; Clay; Feldspar Clay

Material Notes: Minspar™ 4 is a medium particle size, ground Feldspar with a tightly controlled particle size distribution. The small amount of material retained on a 325 mesh screen, in conjunction with excellent exterior durability, make this an excellent candidate for use in low sheen coatings and primers, along with adhesive, sealant, caulk and elastomeric formulations.

Information provided by Imerys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.60 g/cc
Bulk Density 40.0 lb/ft³loose
 60.0 lb/ft³packed
Density 21.6 lb/galsolid
Brightness 91 %G.E. Brightness
Particle Size 8.0 µmmean
Particle Mesh Size 325 Mesh0.05% retained
pH 9.310% solids
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 6.0
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.53
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 0.10 %
 
Descriptive Properties
Hegman Grind4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Imerys Minspar™ 10 Ground Feldspar
Imerys Minspar™ 7 Ground Feldspar
COI Ceramics Sylramic™ S400 Silicon Carbide Ceramic Matrix Composite, Carbon
Imerys Minspar™ 200 Feldspar
Imerys Minspar™ 3 Ground Feldspar

CIMERY008 / 88358

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.