Key Features:- High thermal conductivity
- Superior electrical insulation
- Room temperature curing
- High thermal conductivity
- Superior electrical insulation
- Room temperature curing
Product Description: Master Bond Supreme 11AOHT is a two component epoxy resin system for high performance bonding and sealing. It is formulated to cure at room temperature or more rapidly at elevated temperatures with a convenient one to one mix ratio by weight or volume. Its most outstanding features include high thermal conductivity, excellent electrical insulation properties and temperature resistance up to +400°F. Supreme 11AOHT is a “toughened” system which enables it to withstand rigorous thermal cycling and makes it well suited for bonding dissimilar substrates. It has excellent adhesion to most metals, ceramics, glass and vulcanized rubbers as well as many plastics. Additionally, the toughness imparts high shear and peel strengths. Its chemical resistance profile includes water, oil and fuels. Both Parts A and B are colored off-white. Master Bond Supreme 11AOHT is widely used in electronic, electro-optic, aerospace and specialty applications where high strength, excellent thermal transfer properties, and high temperature resistance are required. Product Advantages: - Convenient one to one mix ratio by weight or volume
- Versatile cure schedules; ambient temperature cures or faster elevated temperature cures as required
- High shear and peel strengths to a wide variety of substrates
- Toughened system, can withstand rigorous thermal Cycling
- High thermal conductivity with exceptional electrical insulation properties
- Thermally stable up to +400°F with good thermal cycling properties
- Exceptionally good dimensional stability
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |