MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Eastman Pamolyn™ 380 Conjugated Linoleic Acid
Categories: Fluid

Material Notes: Product Description: Pamolyn™ 380 conjugated linoleic acid is produced synthetically by an Eastman process that isomerizes 9, 12-linoleic acid to the 9, 11-conjugated form, and controls production of the latter to a uniform ratio of cis-trans to trans-trans isomers. It is a pale, low odor, oily liquid that has excellent heat color stability and an exceptionally low titer. Designed mainly for use in the production of polyfunctional chemical intermediates by Diels-Alder chemistry, Pamolyn™ 380 linoleic acid typically contains 69% conjugated unsaturation. The remaining portion is primarily oleic and nonconjugated linoleic acid.

Application/Uses:

  • Building and Construction
  • Graphic Arts
  • Hot Melt Adhesives
  • Paint and Coatings
  • Solventborne Adhesives
Key Attributes:
  • Exceptionally low titer point
  • High percentage of conjugated linoleic acid
  • Low odor
  • Pale color
  • Uniform ratio of cis-trans to tras-trans isomers

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.910 g/cc0.0329 lb/in³
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 195195
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 2.72.7
 
Descriptive Properties
Colorafter heat test, D 1981-61
Saponification Number197

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5485 / 222679

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.