MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Toray AMILAN™ CM1007 Nylon 6, Unreinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Unreinforced, high flow, PA6.

General Amilan™ Notes: AMILAN™ nylon (polyamide) is a thermoplastic engineering plastic containing an amide group (-CONH-) and it exhibits excellent strength, toughness, heat resistance, and anti-friction wear resistance. A variety of grades designed for various customer needs and applications are available.

Information provided by Toray Resin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccDry; ISO 1183
Water Absorption 10.5 %23°C in water, polymer initally dry; ISO 62
 1.8 %
@Time 86400 sec
In 23°C water, polymer initally dry; ISO 62
Linear Mold Shrinkage, Flow 0.010 - 0.016 cm/cm80x80x3mmt. Dry; Toray Method
Linear Mold Shrinkage, Transverse 0.0050 - 0.010 cm/cm80x80x3mmt. Dry; Toray Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 80
@Temperature 80.0 °C
ISO 2039-2
 90
@Temperature 23.0 °C
ISO 2039-2
 119
@Temperature 23.0 °C
ISO 2039-2
Tensile Strength 20.0 MPa
@Temperature 80.0 °C
3.5% Moisture Content; ISO 527-1,2
 25.0 MPa
@Temperature 80.0 °C
Dry; ISO 527-1,2
 35.0 MPa
@Temperature 23.0 °C
3.5% Moisture Content; ISO 527-1,2
 80.0 MPa
@Temperature 23.0 °C
Dry; ISO 527-1,2
 100 MPa
@Temperature -40.0 °C
3.5% Moisture Content; ISO 527-1,2
 110 MPa
@Temperature -40.0 °C
Dry; ISO 527-1,2
Elongation at Break 35 %Dry; ISO 527-1,2
 50 %3.5% Moisture Content; ISO 527-1,2
Elongation at Yield 2.0 %Dry; ISO 527-1,2
Flexural Strength 25.0 MPa
@Temperature 80.0 °C
3.5% Moisture Content; ISO 178
 40.0 MPa
@Temperature 23.0 °C
3.5% Moisture Content; ISO 178
 40.0 MPa
@Temperature 80.0 °C
Dry; ISO 178
 110 MPa
@Temperature 23.0 °C
Dry; ISO 178
 125 MPa
@Temperature -40.0 °C
3.5% Moisture Content; ISO 178
 135 MPa
@Temperature -40.0 °C
Dry; ISO 178
Flexural Modulus 0.300 GPa
@Temperature 80.0 °C
3.5% Moisture Content; ISO 178
 0.700 GPa
@Temperature 80.0 °C
Dry; ISO 178
 0.800 GPa
@Temperature 23.0 °C
3.5% Moisture Content; ISO 178
 2.80 GPa
@Temperature 23.0 °C
Dry; ISO 178
 3.60 GPa
@Temperature -40.0 °C
3.5% Moisture Content; ISO 178
 3.80 GPa
@Temperature -40.0 °C
Dry; ISO 178
Compressive Strength 80.0 MPaDry; ISO 604
Shear Strength 65.0 MPa3.5% Moisture Content; ASTM D732
 70.0 MPaDry; ASTM D732
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -40.0 °C
V-Notched. Dry; ISO 179
 5.00 kJ/m²
@Temperature 23.0 °C
V-Notched. Dry; ISO 179
 31.0 kJ/m²
@Temperature 23.0 °C
V-Notched. 3.5% Moisture Content; ISO 179
Coefficient of Friction 0.15 - 0.20Vs Metal. Dry. Without lubrication; Suzuki Method
Taber Abrasion, mg/1000 Cycles 3.0 - 4.0Dry; ISO 9352
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cm3.5% Moisture Content; IEC 60093
 1.00e+14 - 1.00e+15 ohm-cmDry; IEC 60093
Dielectric Constant 3.4
@Frequency 1e+6 Hz
60% RH; IEC 60250
 3.9
@Frequency 1000 Hz
60% RH; IEC 60250
 4.1
@Frequency 5000 Hz
60% RH; IEC 60250
 4.5
@Frequency 1e+6 Hz
60% RH. (3.5% Moisture Content); IEC 60250
 8.0
@Frequency 1000 Hz
60% RH. (3.5% Moisture Content); IEC 60250
 9.0
@Frequency 5000 Hz
60% RH. (3.5% Moisture Content); IEC 60250
Dielectric Strength 508 V/milDry; IEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
60% RH; IEC 60250
 0.060
@Frequency 1000 Hz
60% RH; IEC 60250
 0.070
@Frequency 5000 Hz
60% RH; IEC 60250
 0.10
@Frequency 5000 Hz
60% RH. (3.5% Moisture Content); IEC 60250
 0.11
@Frequency 1000 Hz
60% RH. (3.5% Moisture Content); IEC 60250
 0.13
@Frequency 1e+6 Hz
60% RH. (3.5% Moisture Content); IEC 60250
Arc Resistance 120 secTungsten Electrode. Dry; UL-746A
Comparative Tracking Index 600 VDry; UL 746B
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°CDry; ISO 11359-2
Specific Heat Capacity 1.90 J/g-°CDry
Thermal Conductivity 0.250 W/m-KDry
Melting Point 225 °CDSC Method
Deflection Temperature at 0.46 MPa (66 psi) 182 °CDry; ISO 75-1,2
Flammability, UL94 V-2
@Thickness 0.800 mm
3.5% Moisture Content
 V-2
@Thickness 0.800 mm
Dry

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTORAY9089 / 248779

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.