MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BNZ Materials Super Blakbond Mortar
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Super Blakbond is an air-setting mortar for general purpose plant use. It has greater air-setting strength than Blakbond or No. 2986. It is good for insulating fire brick where greater bond strength is desired, and can also be used for dense fire brick. Super Blakbond is particularly good for deep patching. It is also used for coating over industrial boiler tubes to level the surface and for shallow patching. The overall excellent properties of Super Blakbond make it ideal for the one mortar to carry in plant inventory. Temperature to 3000°F. An excellent choice for the one mortar on a job involving dense fire brick and insulating fire brick.

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 124 lb/ft³Dipping, 4% H2O
 126 lb/ft³As received
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00259 GPaDipped Joint; ASTM C198
 0.0290 GPaMortar
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 3000 °F
Shrinkage 4.3 %Permanent Linear Change at Use Limit
 
Component Elements PropertiesOriginal ValueComments
Al2O3 43.2 %
CaO 0.30 %
Fe2O3 1.2 %
K2O 0.80 %
Loss on Ignition(%) 1.8 %
Na2O 2.4 %
SiO2 48.8 %
TiO2 1.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast FSC-2000 Stabilized fused silica cement
Chosun Refractories SM-1 Special Mortar
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work

CBNZ955 / 149195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.