MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kumho-Sunny HNB0225G4M PA6/ABS, 20/20% Glass/Mineral Reinforced
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced

Material Notes: PA/ABS HNB0225G4M is a 20% glass fiber & 20% mineral reinforced PA6/ABS blend with excellent dimensional stability, high impact strength and good antistatic property.

Features: Good antistatic property; Excellent dimensional stability

Application: Air vent vane

Information provided by Shanghai Kumho Sunny Plastics co, Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cmISO 294
Melt Flow 38 g/10 min
@Load 10.0 kg,
Temperature 240 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 83.0 MPa50mm/min; ISO 527
Flexural Strength 120 MPa2mm/min; ISO 178
Flexural Modulus 5000 MPa2mm/min; ISO 178
Charpy Impact, Notched 6.00 kJ/m²
@Thickness 3.17 mm
4J; ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 110 °C120°C/h; ISO 75
Vicat Softening Point 130 °C
@Load 5.00 kg
50°C/h; ISO 306
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 190 - 210 °C
Middle Barrel Temperature 210 - 220 °C
Front Barrel Temperature 220 - 240 °C
Nozzle Temperature 230 - 250 °C
Melt Temperature 230 - 250 °C
Mold Temperature 60.0 - 90.0 °C
Drying Temperature 80.0 - 90.0 °C
Dry Time 3.00 - 4.00 hour
 
Descriptive Properties
Flammability=80 mm/min360*100*3 mm, ISO 3795

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKMSN192 / 281044

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.