MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Parker Chomerics Tecknit® 73-00025 Electrically Conductive Acrylic and Polyurethane Paint
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS

Material Notes: Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosures, which are susceptible to EMI, and other applications requiring a flexible protective shield.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1.0 ohm<= 1.0 ohmCured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 134 °C273 °FCured
Minimum Service Temperature, Air -54.0 °C-65.2 °FCured
 
Processing PropertiesMetricEnglishComments
Cure Time 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
Pot Life 30 min
@Temperature 25.0 °C
30 min
@Temperature 77.0 °F
Shelf Life 6.00 Month6.00 MonthUnopened Container
 
Descriptive Properties
ColorSilver Gray
ConsistencyThin Paint
Coverage56 sq. ftRecommended 0.002" thick
FillerAg/Glass
Final ConditionDurable Film
Number of ComponentsOne
ResinAcrylic
Volume16.4 in3
Weight16 oz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME411 / 131121

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.