MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Plastcom SLOVAMID 66 HI Polyamide 66, Impact Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Features

Modified with thermoplastic reactive elastomer, determined for mouldings with high toughness also at low temperatures. Eligible application for ski-shoes, helmets for sport and other safety use /hockey, building/, protection frames of car doors. Withstands high dynamic stress up to -40°C. Delivered in natural and in the full RAL color scale.

Application: Injection Moulding

Information Provided by Plastcom spol. s r.o.

Key Words: PA66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³STN 64 0111
Linear Mold Shrinkage 0.018 cm/cm0.018 in/inSTN 64 0808
Linear Mold Shrinkage, Transverse 0.0183 cm/cm0.0183 in/inSTN 64 0808
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiSTN EN ISO 527-2
Elongation at Break 50 %50 %STN EN ISO 527-2
Tensile Modulus 1.80 GPa261 ksiSTN EN ISO 527-2
Flexural Strength 60.0 MPa8700 psiSTN EN ISO 178
Flexural Modulus 1.50 GPa218 ksiSTN EN ISO 178
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
STN EN ISO 179
 NB
@Temperature -20.0 °C
NB
@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched  1.00 J/cm²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
STN EN ISO 179
 1.20 J/cm²
@Temperature 23.0 °C
5.71 ft-lb/in²
@Temperature 73.4 °F
STN EN ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 59.0 °C138 °FSTN EN ISO 75/A
Vicat Softening Point 190 °C374 °FB; STN EN ISO 306
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.15 %0.15 %STN EN ISO 960
Injection Pressure 70.0 - 120 MPa10200 - 17400 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 MI LS PA66, improved strength
E-Polymers TEKAMID® TA210ST Super Tough PA66, DAM
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Plastcom SLOVAMID 66 MI PA66, improved strength
Plastcom SLOVAMID 66 SHI PA66, improved strength

PPLACO040 / 106918

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.