MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Nouryon Trigonox 42S Thermoset tert-Butyl peroxy-3,5,5-trimethylhexanoate
Categories: Other Engineering Material

Material Notes: Trigonox 42S is an initiator for (co)polymerization of ethylene, styrene, acrylonitrile acrylates and (meth)acrylates.

CAS number: 13122-18-4

EINECS/ELINCS No: 236-050 7

Applications: For Polymer Production: Polymerization of ethylene: Trigonox 42S is an efficient initiator for the ethylene polymerization under high pressure in both autoclave and tubular processes. To obtain a wide spectrum of polymerization temperatures, combinations with other peroxides are applied in practice. Depending on reaction conditions, Trigonox 42S is active in the temperature range of 210-240°C. Polymerization of acrylates and methacrylates: Trigonox 42S can be used as initiator for the solution (co)polymerization of acrylates and methacrylates in the temperature range of 90-175°C, amongst others for the manufacture of coatings. Trigonox 42S can also be applied as an initiator for the bulk and suspension (co)polymerization of acrylates and methacrylates in the temperature range of 90-130°C. Polymerization of styrene: Trigonox 42S may be used for the (co)polymerization of styrene in the temperature range of 90-140°C. For Thermoset: Trigonox 42S, tert-butylperoxy-3,5,5-trimethylhexanoate, is a perester which is used for the curing of unsaturated polyester resins at elevated temperatures. Trigonox 42S is preferred for the curing of UP resin based Hot Press Moulding formulations (SMC, DMC, BMC etc.) in the temperature range of 120 - 170°C. In combination with a cobalt accelerator (e.g. Accelerator NL-53N, 10% cobalt) Trigonox 42S is also applicable for the cure of UP resins in the temperature range of 70°C and higher. Application area can be air drying lacquers, diplacquers, filament winding etc. Trigonox 42S has in comparison with Trigonox C, tert-butylperbenzoate, a somewhat higher reactivity in the pure resin as well as in HPM formulations.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³
Half-life  0.100
@Temperature 135 °C
0.100
@Temperature 275 °F
[hr]
 1.00
@Temperature 114 °C
1.00
@Temperature 237 °F
[hr]
 10.0
@Temperature 94.0 °C
10.0
@Temperature 201 °F
[hr]
Viscosity 5.0 cP5.0 cP
Molecular Weight 230.3 g/mol230.3 g/mol
Storage Temperature -20.0 - 25.0 °C-4.00 - 77.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 55.0 °C131 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceClear liquid
Assay= 97.0 %
Color<50 Pt-Co / APHA
Content=150 mg/kgInorganic + organic hydrolysable chloride
 0.001Hydroperoxides as TBHP
 6.74%Active oxygen
Content (%)6.95Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1125 / 286648

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.