MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Phosphor bronze 8% Sn, UNS C52100, H02 Temper rod
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Good cold workability for blanking, drawing, forming and bending, shearing and stamping.

Applications: more severe service conditions than C51000.

Trace content of Phosphorus.

Test specimen: rod - 13mm diameter.

Key Words: CDA 521, PB104, ISO CuSn8P
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 85
Tensile Strength, Ultimate 550 MPa
Tensile Strength, Yield 450 MPa
Elongation at Break 33 %in 50 mm
Modulus of Elasticity 110 GPa
Poissons Ratio 0.341
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 41.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000133 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 62.0 W/m-K
@Temperature 20.0 °C
Melting Point 880 - 1025 °C
Solidus 880 °C
Liquidus 1025 °C
Annealing Point 900 - 1250 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 475 - 675 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 90.5 - 92.8 %
Iron, Fe <= 0.10 %
Lead, Pb <= 0.050 %
Phosphorus, P 0.030 - 0.35 %
Tin, Sn 7.0 - 9.0 %
Zinc, Zn <= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO35 Temper rod
Phosphor bronze 5% Sn, UNS C51000, H02 Temper 25 mm rod
Phosphor bronze 8% Sn, UNS C52100
Phosphor bronze 1.25% Sn, UNS C50500, H10, 0.015 mm Grain Size
Phosphor bronze 1.25% Sn, UNS C50500, H10, 0.035 mm Grain Size

MC52100c4 / 11545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.