MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carmel Olefins Ipethene® 100 Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: IPETHENE® 100 is a low density polyethylene extrusion grade. It exhibits good impact and puncture resistance, good processability and good ESCR.

APPLICATIONS

IPETHENE® 100 is used for production of irrigation pipe systems, 80 to 250 µm films for heavy duty and shrink packaging, greenhouses, net coverings, and industrial applications. Other extrusion applications are pipe systems, sheets, tubes, bottles, containers, nets and various profiles.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/ccISO 1183-A
ESCR 10% Igepal® 18 hourF50; ASTM D1693
Thickness 100 microns
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 350 %ISO 1184
Film Elongation at Break, TD 450 %ISO 1184
Elmendorf Tear Strength MD 300 gISO 6283-2
Elmendorf Tear Strength TD 500 gISO 6283-2
Elmendorf Tear Strength, MD 3.00 g/micronISO 6283-2
Elmendorf Tear Strength, TD 5.00 g/micronISO 6283-2
Dart Drop 6.30 g/micronF50; ISO 7765-A
Dart Drop Test 630 gF50; ISO 7765-A
Film Tensile Strength at Break, MD 22.0 MPaISO 1184
Film Tensile Strength at Break, TD 19.0 MPaISO 1184
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 °C
Blow-up Ratio (BUR) 2.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carmel Olefins Ipethene® 4203 Low Density Polyethylene
SCG Chemicals EL-Lene™ D682PC Low Density Polyethylene Pipe Resin
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes
Braskem Green PE SLL118 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene
Breplast Bretene LD PIPE Low Density Polyethylene

PCARM002 / 79740

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.