MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASI® FLEX 1100 Silicone Adhesive/Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: FLEX 1100 is a multi-purpose silicone for use in numerous bonding and sealing applications. Designed primarily for flange sealing with good oil resistance and to withstand high joint-movement requirements. For example, stamped sheet metal covers (timing covers and oil sumps).

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/cc
@Temperature 20.0 °C
uncured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35ASTM D2240
Tensile Strength >= 203 psiASTM D412
Elongation at Break >= 400 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 6.70e+13 ohm-cmASTM D257
Surface Resistance 4.35e+15 ohmASTM D257
Dielectric Constant 4.12
@Frequency 1e+7 Hz
ASTM D150
 4.13
@Frequency 1e+6 Hz
ASTM D150
 4.29
@Frequency 100000 Hz
ASTM D150
 5.05
@Frequency 1000 Hz
ASTM D150
Dielectric Loss Index 0.013
@Frequency 1e+7 Hz
ASTM D150
 0.023
@Frequency 1e+6 Hz
ASTM D150
 0.042
@Frequency 100000 Hz
ASTM D150
 0.048
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °Cuncured
 
Processing PropertiesOriginal ValueComments
Extrusion Rate 35.0 g/min
@Pressure 0.600 MPa,
Temperature 25.0 °C
3mm nozzle. Uncured
 
Descriptive Properties
Chemical ClassAcetoxy Silicone
Color / appearanceRubber paste
ViscosityThixotropic paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9218 / 233584

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.