MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chesterton 783 ACR Anti-Seize Compound
Categories: Fluid; Lubricant

Material Notes: A proprietary blend of ultra-fine inorganic solid lubricants, 783 ACR can be used under extremely severe conditions of temperature and pressure to assist in assembly and disassembly of threaded components. 783 ACR can be used over a broad temperature range. Hardening will not occur when used between -34°C to 900°C (-30°F to 1650°F).

Features:

  • No Toxic Heavy Metals
  • For Extreme Pressure= up to 8928 kg/cm2 (126,983 psi)
  • Broad Service Temperature Range
  • Ultra-Fine Particles
  • Corrosion Resistant
  • Waterproof

Benefits:

  • Safer to workers
  • Usable under most extreme conditions
  • Fills in microscopic voids

Suggested Uses: Bolts, screws, studs, pipe threads, press fits, pump sleeves and splines. Use in power plants, textiles mills, bakeries, foundries, steel mills, boiler rooms, oil refineries, marine applications, chemical plants, automotive industry.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/cc
Particle Size <= 11 µm<= 11 µm
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Load Wear Index 168.7168.7127,000 psi; ASTM D2596, DIN 51 350
Four Ball Extreme Pressure, Weld Load 800 kg1760 lb (mass)ASTM D2596, DIN 51 350
Penetration 270270ASTM D217, ISO2137
K Factor (Wear Factor) 0.140.14Skidmore - Wilhelm Method
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 900 °C1650 °F
Minimum Service Temperature, Air -34.0 °C-29.2 °F
Dropping Point >= 288 °C>= 550 °FASTM D566, ISO2176
 
Descriptive Properties
ColorLight gray
Consistency2NLGI
 Soft Paste
Copper Corrosion2A24 hrs. @ 100°C (212°F), ASTM D4048, DIN 51 811
Corrosion Resistance>1200 hrs.@ 100 microns, 5% NaCl, ASTM B117
Water Washout Resistance<0.13%@ 79°C, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS093 / 138205

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.