MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Arkema Rilsamid® ASR 20 PA12-CF20
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: Property data for dry samples, unless noted.

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Melt Flow 10 g/10 min
@Load 5.00 kg,
Temperature 235 °C
MVR (cm³/10min); ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 128 MPaConditioned; ISO 527-1/-2
 132 MPaISO 527-1/-2
Elongation at Break 4.0 %Conditioned; ISO 527-1/-2
 5.0 %ISO 527-1/-2
Tensile Modulus 11435 MPaConditioned; ISO 527-1/-2
 12580 MPaISO 527-1/-2
Charpy Impact Unnotched 58.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 59.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 59.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 64.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 17.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 17.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6.0 ohm-cmConditioned; IEC 60093
Dielectric Strength 1.00 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 100 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 175 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 160 °CISO 75-1/-2
Vicat Softening Point 170 °C50°C/h 50N; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695-11-10
 HB
@Thickness 3.20 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 °CInjection Molding; ISO 294
Mold Temperature 60.0 °CInjection Molding; ISO 10724
Hold Pressure 19.0 MPaInjection Molding; ISO 294
 
Descriptive Properties
FeaturesAnti-static
 Heat stabilized or stable to heat
 Increased electrical conductivity
 Light stabilized or stable to light
 UV stabilized or stable to weather
FormPellets
Processing MethodsInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® L 20 W 20 PA12
EMS-Grivory Grilamid® TR 55 LY PA12/MACMI
Akro-Plastic Akromid® A3 GF 25 1 L black (4672) PA66 + PP, Dry, 25% Glass Filled
Celanese Vectra® C115 Liquid Crystal Polymer (LCP), 15% Glass Reinforced
EMS-Griltech Grilamid® DN 80 Nylon 12 Monofilament

PZARKF863 / 193611

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.