MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F149 1581 Vacuum, Glass Reinforcement, Polyester Resin System
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Description: HexPly® F149 is a structural and electrical grade polyester resin system. It is self-extinguishing and exhibits high laminate strengths. HexPly® F149 can be tailored to any tack and drape, and cures at relatively low temperatures and pressures. It is a good oven cure type prepreg.

Benefits and Features

  • 250°F (121°C) Cure
  • Vacuum Bag, Autoclave, or Press Cure
  • Service Temperature up to 300°F (149°C)
  • Meets Requirements of MIL-R-7575C, Grades A and B, Class 0 and 4

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 70.070.0
Tensile Strength 345 MPa50000 psiWet
 359 MPa52000 psiDry
Tensile Modulus 21.4 GPa3100 ksiWet
 22.1 GPa3200 ksiDry
Flexural Strength 469 MPa68000 psiWet
 483 MPa70000 psiDry
Flexural Modulus 22.1 GPa3200 ksiWet
 22.8 GPa3300 ksiDry
Compressive Strength 331 MPa48000 psiWet
 359 MPa52000 psiDry
Compressive Modulus 22.8 GPa3300 ksiWet
 23.4 GPa3400 ksiDry
Shear Strength 21.4 MPa3100 psiShort Beam, Wet
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.25
@Frequency 8.50e+9 - 1.00e+10 Hz
4.25
@Frequency 8.50e+9 - 1.00e+10 Hz
Dry
 4.33
@Frequency 8.50e+9 - 1.00e+10 Hz
4.33
@Frequency 8.50e+9 - 1.00e+10 Hz
Wet
Dielectric Loss Index  0.0110
@Frequency 8.50e+9 - 1.00e+10 Hz
0.0110
@Frequency 8.50e+9 - 1.00e+10 Hz
Dry
 0.0150
@Frequency 8.50e+9 - 1.00e+10 Hz
0.0150
@Frequency 8.50e+9 - 1.00e+10 Hz
Wet
 
Processing PropertiesMetricEnglishComments
Shelf Life  1.00 Month
@Temperature 21.0 °C
1.00 Month
@Temperature 69.8 °F
 3.00 Month
@Temperature 4.00 °C
3.00 Month
@Temperature 39.2 °F
 6.00 Month
@Temperature -18.0 °C
6.00 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9189 / 322345

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.