MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-temperature flexibility.

    PEARLCOAT® 125K is used in a wide range of applications:
  • Melt coatings on textile substrates, for conveyor belts, belting, among other end uses, obtained by extrusion, calendering or sintering (in this last case the product is previously ground, so as to be in powder form);
  • Extruded films and fabric coatings;
  • Low melting point carrier for TPU color and additives masterbatches.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Tensile Strength, Yield 30.1 MPa4360 psiASTM D412
Elongation at Break 500 %500 %ASTM D412
50% Modulus 5.00 MPa
@Strain 50 %
5.00 MPa
@Strain 50 %
ISO 527-2/5A/500
100% Modulus 6.00 MPa
@Strain 100 %
870 psi
@Strain 100 %
ASTM D412
300% Modulus 9.018 MPa
@Strain 300 %
1308 psi
@Strain 300 %
ASTM D412
Tear Strength 76.0 kN/m434 pliUnnicked; ISO 34-1B
Abrasion 2525Abrasion (mm³); ISO 4649-A
 
Processing PropertiesMetricEnglishComments
Drying Temperature 90.0 °C194 °F
Dry Time 3.00 hour3.00 hour
Dew Point -40.0 °C-40.0 °F
 
Descriptive Properties
Roll 1150°C
Roll 2160°C
Rubber Roll 3not heated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® R185A Thermoplastic Polyurethane
NEU NEUSoft™ 455-60A Ester/ether TPU / SBC blend
NEU NEUSoft™ 602-60A Ester TPU / SBC blend
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
Lubrizol Estane® S168D Thermoplastic Polyurethane

PMES73 / 88450

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.