MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP42HT-2ND-2 Two component epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Convenient mix ratio
  • Long working life
  • Good chemical resistance
  • Paste consistency
Product Description: Master Bond EP42HT-2ND-2 is a room temperature curable two component epoxy, adhesive, sealant, and coating. It has an easy to use 100 to 40 mix ratio by weight or 100 to 50 by volume. It withstands high temperatures along with excellent chemical resistance. It is notable for its high glass transition temperature. The system cures readily at ambient temperatures or more quickly at elevated temperatures. The optimum cure is 8-12 hours at 75°F followed by 2-4 hours at 175-250°F. EP42HT-2ND-2 has good dimensional stability and low shrinkage upon curing. This compound bonds well to a wide variety of substrates including metals, glass, ceramics, plastics, and many rubbers. The cured epoxy has outstanding chemical resistance to various acids, bases, solvents and hydrocarbons. EP42HT-2ND-2 is also a superb electrical and thermal insulator. The service temperature range is from -60°F to 450°F. The color of both Part A and Part B is amber. EP42HT-2ND-2 is an exceptionally versatile system with potential applicability in aerospace, electronic, and specialty OEM, among other high tech industries.

Product Advantages:

  • Non-critical 100:40 mix ratio by weight or 100:50 by volume
  • Outstanding physical strength properties
  • Excellent chemical resistance to acids, alkalis and many solvents
  • Superior thermal stability; serviceable up to 450°F
  • Good gap filler

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80 - 90
Tensile Strength 10000 - 11000 psi
Tensile Modulus 400000 - 450000 psi
Adhesive Bond Strength 1600 - 1800 psiTensile lap shear, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cm
Dielectric Constant 4.4
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 35.0 - 40.0 µm/m-°C
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -60.0 °F
Glass Transition Temp, Tg 150 - 155 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 93.3 °C
 8.00 - 12.0 hour
@Temperature 23.9 °C
Optimum cure, plus 2-4 hours at 175-250°F
 48.0 - 72.0 hour
@Temperature 23.9 °C
Working Life 45.0 - 60.0 minafter mixing, 100 gram batch
Shelf Life 6.00 - 12.0 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio100:40 by weightPart A to B
 100:50 by volumePart A to B
ViscositypastePart A
 pastePart B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM5928 / 306817

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.