MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Proto3000 Ti64 MIM - ASTM F2885 As-Sintered
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Ti64 is ideal for prototyping medical devices such as tweezers, forceps, clamps, suture instruments as well as for 3D printing specialty automotive components, including connecting rods and gearboxes for racing. Its material properties are well known to be a high strength-to-weight ratio and corrosion resistance.

Applications:

  • Automotive
  • Consumer Goods
  • Connecting Rods
  • Sporting Goods
  • Medical Devices
  • Jewelry

Property data per ASTM F2885

Information provided by Proto3000

Key Words: UNS R56400
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 4.25 g/cc
Porosity <= 4.00 %ASTM B311
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 780 MPaASTM E8M
Tensile Strength, Yield >= 680 MPaASTM E8M
Elongation at Break >= 10.0 %ASTM E8M
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 5.50 - 6.75 %
Titanium, Ti 88.75 - 91.0 %Balance
Vanadium, V 3.50 - 4.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NPROTO892 / 322905

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.