MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 954-2A Curing Cyanate Resin, S-2 Glass Fiber Reinforced 8 Harness Satin Fabric
Categories: Polymer; Thermoset; Epoxy

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 627 MPa
@Temperature 23.0 °C
90900 psi
@Temperature 73.4 °F
Elongation at Yield 2.8 %
@Temperature 23.0 °C
2.8 %
@Temperature 73.4 °F
Tensile Modulus 28.3 GPa
@Temperature 23.0 °C
4100 ksi
@Temperature 73.4 °F
Flexural Yield Strength 848 MPa
@Temperature 23.0 °C
123000 psi
@Temperature 73.4 °F
Flexural Modulus 28.3 GPa
@Temperature 23.0 °C
4100 ksi
@Temperature 73.4 °F
Compressive Yield Strength  317 MPa
@Temperature 163 °C
46000 psi
@Temperature 325 °F
0°, Wet
 345 MPa
@Temperature 149 °C
50000 psi
@Temperature 300 °F
0°, Wet
 365 MPa
@Temperature 204 °C
52900 psi
@Temperature 399 °F
 379 MPa
@Temperature 191 °C
55000 psi
@Temperature 376 °F
 427 MPa
@Temperature 177 °C
61900 psi
@Temperature 351 °F
 434 MPa
@Temperature 163 °C
62900 psi
@Temperature 325 °F
 586 MPa
@Temperature 23.0 °C
85000 psi
@Temperature 73.4 °F
Compressive Modulus  29.0 GPa
@Temperature 191 °C
4210 ksi
@Temperature 376 °F
 29.6 GPa
@Temperature 163 °C
4290 ksi
@Temperature 325 °F
 29.6 GPa
@Temperature 204 °C
4290 ksi
@Temperature 399 °F
 29.6 GPa
@Temperature 23.0 °C
4290 ksi
@Temperature 73.4 °F
 31.0 GPa
@Temperature 177 °C
4500 ksi
@Temperature 351 °F
Shear Strength  35.2 MPa
@Temperature 163 °C
5110 psi
@Temperature 325 °F
Short Beam, Wet
 37.2 MPa
@Temperature 204 °C
5400 psi
@Temperature 399 °F
Short Beam
 37.2 MPa
@Temperature 149 °C
5400 psi
@Temperature 300 °F
Short Beam, Wet
 41.4 MPa
@Temperature 177 °C
6000 psi
@Temperature 351 °F
Short Beam
 43.4 MPa
@Temperature 191 °C
6290 psi
@Temperature 376 °F
Short Beam
 52.4 MPa
@Temperature 163 °C
7600 psi
@Temperature 325 °F
Short Beam
 75.2 MPa
@Temperature 23.0 °C
10900 psi
@Temperature 73.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-3 Curing Cyanate Resin
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
CRG Industries Advantic™ 30 Syntactic Foam
CRG Industries Advantic™ 40 Syntactic Foam
Hexcel® HexPly® 954-3A Curing Cyanate Resin

PHEXC023 / 98493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.