MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Global B-5200 High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description-has excellent stiffness thus requires less material to make blow molding
Applications-food containers, drinking bottles, medicine bottles, water containers

Information provided by Global Polymers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.966 g/ccASTM D1505
Environmental Stress Crack Resistance 40 hourASTM D1693
Melt Flow 0.35 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240
Tensile Strength, Ultimate 350 kg(f)/cm²ASTM D638
Tensile Strength, Yield 320 kg(f)/cm²ASTM D638
Elongation at Break 500 %ASTM D638
Flexural Modulus 11000 kg(f)/cm²Olsen Stiffness; ASTM D747
Izod Impact, Notched 50.0 kg-cm/cmASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 134 °CASTM D2117
Vicat Softening Point 128 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Petromont 8001 High Density Polyethylene Resin
Global B-8200 High Density Polyethylene
Petromont 5001 High Density Polyethylene Resin
Braskem BU004 Blow Molding High Density Polyethylene
Borealis BL2631 High Density Polyethylene

PGLOBE09 / 42058

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.