MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

LyondellBasell Alathon® H4557X02 High Density Polyethylene, Injection Molding Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: ALATHON H4557X02 is a high-flow freezer grade resin that exhibits enhanced cold temperature impact performance, enhanced processability and thermal stability, with good color and organoleptic properties. Typical applications are rigid food containers such as four, five, and sixquart ice cream containers that are produced at high speeds in fast cycling multi-cavity stack molds.

Regulatory Status: H4557X02 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D1505
Melt Flow 57 g/10 min57 g/10 minASTM D1238
Spiral Flow 45.7 cm18.0 inEquistar test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363ASTM D2240
Tensile Strength at Break 22.7 MPa3290 psi2"/min; ASTM D638
Flexural Modulus, 1% Secant 889 MPa129000 psi0.5"/min; ASTM D790
2% Secant Modulus 0.765 GPa111 ksi0.5"/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °C145 °FASTM D648
Vicat Softening Point 118 °C244 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 232 °C450 °F
Middle Barrel Temperature 243 °C470 °F
Front Barrel Temperature 246 °C475 °F
Nozzle Temperature 246 °C475 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® M6028 High Density Polyethylene
Entec Hypel® PEHD32/.951 HDPE
Entec Hypel® PEHD30/.950 HDPE
Entec Hypel® PEHD20/.953 HDPE
Entec Hypel® PEHD18/.956 HDPE

PEQU0788 / 104144

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.