MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Multifak® EP NLGI Grade 1
Categories: Fluid; Lubricant; Lithium Gellant

Material Notes: Texaco Multifak EP greases deliver value through:
  • Good water resistance — Strong resistance to wash out of bearings.
  • Good rust and corrosion protection, even in wet conditions.
  • Extreme pressure protection.
  • Protection against shock loading, thus extending bearing life.
  • Outstanding film strength.
  • Good low temperature pumpability — Better handling in the container and grease dispensing equipment.

Texaco Multifak EP greases are water resistant, extreme pressure, heavy duty chassis, wheel bearing and general purpose lubricating greases.

They are manufactured using highly refined, select high viscosity index base oils, and a lithium soap. They are brown in color and smooth and buttery in texture.

Texaco Multifak EP greases are available in three grades:

  • NLGI 0, 1 for better pumpability at low ambient temperatures.
  • NLGI 2 for use in normal ambient temperatures.

Texaco Multifak EP greases are formulated to:

  • Protect bearings and other metal surfaces from corrosion when exposed to wet conditions.
  • Resist water. These greases strongly resist being washed out of bearings.
  • Retain their consistency under adverse service conditions.
  • Provide outstanding film strength and adhesive properties. As a result, Texaco Multifak EP greases are particularly effective in providing low wear in shock load service.
  • Operate effectively over a wide temperature range.

Texaco Multifak EP greases are recommended for:
  • General use in the lubrication of trucks, tractors, and passenger cars. This includes ball joints, universal joints, and all other chassis points, non-disc brake wheel bearings, water pumps, and fifth wheels.
  • Boat trailer wheel bearings.

Texaco Multifak EP 2 is approved for the NLGI Certification Mark LB.

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Notes:

  1. Minimum operating temperature is the lowest temperature at which a grease, already in place, could be expected to provide lubrication. Most greases cannot be pumped at these minimum temperatures.
  2. Maximum operating temperature is the highest temperature at which the grease could be used with frequent (daily) relubrication.
  3. Determined on mineral oil extracted by vacuum filtration.

CPS Number: 220921; MSDS Number: 8644

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 9090Viscosity Index, See Note 3.
Saybolt Viscosity at 100°F 914 SUS914 SUSSee Note 3.
Saybolt Viscosity at 210°F 82 SUS82 SUSSee Note 3.
Kinematic Viscosity at 40°C (104°F) 173 cSt173 cStSee Note 3.
Kinematic Viscosity at 100°C (212°F) 15.6 cSt15.6 cStSee Note 3.
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 315 kg695 lb (mass)
Four Ball Wear 0.500 mm0.0197 inScar Diameter
Penetration P(0), 1/10 mm 305305Unworked, 25°C (77°F)
Penetration P(60), 1/10 mm 325325Unknown Amount of Work, 25°C (77°F)
Timken Test 18100 g40.0 lbOK Load
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FSee Note 2.
Minimum Service Temperature, Air -34.0 °C-29.2 °FSee Note 1.
Pour Point -12.0 °C10.4 °FSee Note 3.
Flash Point 198 °C388 °FSee Note 3.
Dropping Point 186 °C367 °F
 
Descriptive Properties
ColorBrown
TextureButtery
Thickener, %9Lithium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MetalTek MTEK CA6NM Cast UNS J91540 Martensitic Stainless Steel
Cast Stainless Steel E3N, ASTM A757

WTEXA257 / 77136

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.