System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound PFL26 Polyamide 6 (Nylon 6)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
Material Notes:
LNP LUBRICOMP PFL26 compound is based on Nylon 6 resin containing 30% glass fiber, 10% PTFE. Added features of this grade include: Wear Resistant
Features: Wear resistant,Structural
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.44
g/cc
0.0520
lb/in³
ISO 1183
Moisture Absorption
0.150 - 0.250 %
0.150 - 0.250 %
Injection Molding
Linear Mold Shrinkage, Flow
0.0010
-
0.0030
cm/cm
0.0010
-
0.0030
in/in
SABIC method
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
250
MPa
36300
psi
5 mm/min; ISO 527
Elongation at Break
4.2 %
4.2 %
5 mm/min; ISO 527
Tensile Modulus
10.2
GPa
1480
ksi
1 mm/min; ISO 527
Flexural Strength
165
MPa
23900
psi
break, 2mm/min; ISO 178
Flexural Modulus
8.60
GPa
1250
ksi
2 mm/min; ISO 178
Flexural Strain at Break
3.9 %
3.9 %
2 mm/min; ISO 178
Izod Impact, Notched (ISO)
14.0
kJ/m²
6.66
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
98.0
kJ/m²
46.6
ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic
0.57
0.57
ASTM D3702 Modified: Instr.
Coefficient of Friction, Static
0.99
0.99
ASTM D3702 Modified: Instr.
K (wear) Factor
20.1
x 10
-8
mm³/N-M
10.0
x 10
-10
in³-min/ft-lb-hr
Washer; ASTM D3702 Modified: Instr.
Electrical Properties
Metric
English
Comments
Comparative Tracking Index
400
-
600
V
400
-
600
V
UL 746A
Hot Wire Ignition, HWI
60
-
120
sec
@Thickness >=1.50 mm
60
-
120
sec
@Thickness >=0.0591 in
UL 746A
>=
120
sec
@Thickness >=2.50 mm
>=
120
sec
@Thickness >=0.0984 in
UL 746A
High Amp Arc Ignition, HAI
>=
120
arcs
@Thickness >=1.50 mm
>=
120
arcs
@Thickness >=0.0591 in
UL 746A
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
24.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
13.3
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow
75.0
µm/m-°C
@Temperature 23.0 - 60.0 °C
41.7
µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
219
°C
426
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi)
206
°C
403
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical
65.0
°C
149
°F
UL 746B
UL RTI, Mechanical with Impact
65.0
°C
149
°F
UL 746B
UL RTI, Mechanical without Impact
65.0
°C
149
°F
UL 746B
Flammability, UL94
HB
@Thickness >=1.50 mm
HB
@Thickness >=0.0591 in
UL 94
Processing Properties
Metric
English
Comments
Zone 2
280
-
295
°C
536
-
563
°F
Zone 3
295
-
305
°C
563
-
581
°F
Melt Temperature
280
-
305
°C
536
-
581
°F
Injection Molding
Mold Temperature
95.0
-
110
°C
203
-
230
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
29.0
-
43.5
psi
Screw Speed
30
-
60
rpm
30
-
60
rpm
Descriptive Properties
UV-light, water exposure/immersion
F1
UL 746C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH80937 / 288884
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.