MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman EastaPure™ EB Solvent
Categories: Fluid; Solvent

Material Notes: Product Description: Eastman EastaPure™ EB solvent is a high flash point, water miscible, colorless solvent providing slow evaporation rate and good viscosity control for a broad range of polymers, resins and coatings. It is primarily used in the production of electronic components in the etching and photoresist processes. Miscible with most organic solvents and water, EastaPure™ EB solvent enables formulators to develop customized blends that meet the most demanding requirements for electronic chemicals in wet processing and photoresist applications. The chemical substances for this product are listed as Inert Ingredients Permitted for Use in Nonfood Use Pesticide Products, and in Food Use Pesticide Products with limitations, under the Federal Insecticide, Fungicide, and Rodenticide Act (FIFRA).

Application/Uses:

  • Advanced resist
  • Developers
  • Edge bead removal
  • Flat Panel/LCD
  • LED/OLED
  • Microelectronics
  • Negative tone resist
  • Photolithography
  • Photoresist
  • Photoresist stripper applications
  • Positive tone resist
  • Semiconductors
  • Solvents
Key Attributes:
  • Excellent resin solubility
  • High assay
  • High Purity/Low Trace Metals
  • Inert - Food use with limitations
  • Inert - Nonfood use
  • Viscosity control

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/cc
Viscosity 3.3 cPLiquid
Molecular Weight 118.17 g/mol
Vapor Pressure 0.000789 atm
@Temperature 20.0 °C
 0.00957 atm
@Temperature 55.0 °C
Surface Tension 20 dynes/cmTLV PPM 2014
 26.6 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 32.0 atm
Critical Temperature 326.8 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 92.0 µm/m-°C
Melting Point -75.0 °CFreezing Point
Boiling Point 169 °C@ 760 mm Hg, Initial
 172 °C@ 760 mm Hg, Dry Point
Flash Point 62.0 °CTag Closed Cup
 70.0 °CTag Open Cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4193
 
Descriptive Properties
ColorPT-Co
Fire Point70°C
Upper Limits for Trace Metals100 ppbAluminum
 100 ppbBarium
 100 ppbCadmium
 100 ppbCalcium
 100 ppbChromium
 100 ppbCobalt
 100 ppbCopper
 100 ppbGallium
 100 ppbGermanium
 100 ppbIron
 100 ppbLead
 100 ppbLithium
 100 ppbMagnesium
 100 ppbManganese
 100 ppbNickel
 100 ppbPotassium
 100 ppbSilver
 100 ppbSodium
 100 ppbTitanium
 100 ppbZinc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Maxxam™ PPR-30G Nat Polypropylene Homopolymer (PP Homopolymer)
3M Novec™ 7300 Engineered Fluid

PEATM5142 / 222336

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.