Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 30% Filler by Weight Additive: Heat Stabilizer Features: Heat Stabilized UL File Number: E157318 Appearance: Black Information provided by TP Composites, Inc. |