MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt POLYCOR® 21 X Series Gel Coat
Categories: Polymer; Thermoset

Material Notes: 21X series isophthalic gelcoats are high quality coatings developed for the fiberglass industry. These gelcoats provide quality finishes and deliver good water resistance, gloss retention and weathering. They are shock proof and can support moderated thermal variations. These gelcoats are formulated to meet the requirements of transportation,truck cabs, sanitary applications and boating. For parts with a prolonged contact with water, an NPG/ISO base gelcoat is recommended. 21X series gel coats are ready to use, sag resistant, fast curing and require only the addition of a proper amount of methyl ethyl ketone peroxide to cure. These gelcoats are available in a wide range of eye-appealing colors. Color matching is available on request.

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brookfield Viscosity 9000 - 15000 cP9000 - 15000 cPRVF #4 Spindle @ 20 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 27.8 - 31.1 °C82.0 - 88.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 45.0 - 60.0 min
@Temperature 25.0 °C
0.750 - 1.00 hour
@Temperature 77.0 °F
Lay-up Time; tested @ 1,8% Norox MEKP 925 @ 25°C
Gel Time 8.00 - 17.0 min
@Temperature 25.0 °C
8.00 - 17.0 min
@Temperature 77.0 °F
1,8% Norox MEKP 925 @ 25°C
 
Descriptive Properties
Sag ResistanceGood at 20 mils
Thixotropic Index>42/20 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9257 / 231852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.