MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK ABP 8037TI Acrylate
Categories: Polymer; Adhesive

Material Notes: Appearance: Silver paste

Cure: Heat cure

Product Benefits:

  • Excellent electrical conductivity
  • High thermal conductivity
  • Excellent adhesive strength
  • Stable at high temperatures
  • Hydrophobic
Application: Die attach

Filler Type: Silver

Key Substrates:

  • Wide variety of metals and ceramic surfaces
  • Silver Plated Copper
  • Preplated leadframes (NiPdAu)
LOCTITE ABLESTIK ABP 8037TI silver filled conductive adhesive is recommended for use in the attachment of integrated circuits and components onto metal leadframes and advanced substrates.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 11000 cPUncured, - HA, Spindle 51, speed 5 rpm
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 1300 MPa
@Temperature 250 °C
Cured, Young's
 1600 MPa
@Temperature 200 °C
Cured, Young's
 1700 MPa
@Temperature 300 °C
Cured, Young's
 4100 MPa
@Temperature 100 °C
Cured, Young's
 5900 MPa
@Temperature 150 °C
Cured, Young's
 5900 MPa
@Temperature 25.0 °C
Cured, Young's
 8400 MPa
@Temperature -65.0 °C
Cured, Young's
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000060 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 62.0 µm/m-°CCured, Below Tg
 94.0 µm/m-°CCured, Above Tg
Thermal Conductivity 4.10 W/m-KCured
Glass Transition Temp, Tg 46.0 °CCured, TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 minramp to 175ºC, hold 30 minutes @ 175 °C
 30.0 minramp to 150ºC, hold 30 minutes @ 150 °C, Alternate Cure Schedule
Working Life 24.0 hour
Shelf Life 12.0 Month
@Temperature -40.0 °C
Uncured, from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)<1Cured, Potassium (K+)
 <10Cured, Chloride (Cl-)
 <20Cured, Sodium (Na+)
Shear Strength17.5 kgDie, 120 x 120 mil Si die on PPF LF @ 25°C
 17.6 kgDie, 120 x 120 mil Ag/Cu LF @ 25°C
 6.9 kgDie, 120 x 120 mil Si die on PPF LF @ 270°C
 7.4 kgDie, 120 x 120 mil Ag/Cu LF @ 270°C
Thixotropic Index2.8Uncured, 0.5/5 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5040 / 255251

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.