MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuBois Polyquench 10 Water-Based Quenchant
Categories: Fluid; Quenchant

Material Notes: Solution of relatively low molecular weight organic polymer, corrosion inhibitors, biocide and anti-foaming agent. The polymer is inversely soluble above 160°F. Typical concentration is 15%.

Information provided by Heatbath Corporation - Park Metallurgical.

Heatbath/Park has been acquired by DuBois Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Saybolt Viscosity at 100°F 1.6 SUSAt 100°F in SUS; cSt
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °FUpper limit of working range
Minimum Service Temperature, Air 80.0 °FLower limit of working range

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik TEGO® Antifoam D 2315 Additive
Evonik TEGO® Antifoam AS 10 Emulsion
Evonik TEGO® Antifoam 793 Defoamer
Evonik TEGO® Antifoam 7001 Defoamer
Evonik TEGO® Antifoam 5-27 Emulsion

WHEATB21 / 75976

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.