MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Polyphenylene Ether, 10% Glass Filled
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 10% Glass Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.10 - 1.30 g/ccAverage value: 1.15 g/cc Grade Count:28
Filler Content 10.0 %Average value: 10.0 % Grade Count:3
Water Absorption 0.0500 - 0.500 %Average value: 0.141 % Grade Count:11
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cmAverage value: 0.00428 cm/cm Grade Count:26
Linear Mold Shrinkage, Transverse 0.00300 - 0.00800 cm/cmAverage value: 0.00472 cm/cm Grade Count:10
Melt Flow 1.00 - 45.0 g/10 minAverage value: 14.0 g/10 min Grade Count:16
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 41.4 - 96.0 MPaAverage value: 75.3 MPa Grade Count:22
 15.0 - 60.0 MPa
@Temperature 60.0 - 120 °C
Average value: 36.7 MPa Grade Count:1
Tensile Strength, Yield 63.8 - 167 MPaAverage value: 85.6 MPa Grade Count:10
Elongation at Break 1.00 - 12.0 %Average value: 4.83 % Grade Count:26
 3.50 - 4.50 %
@Temperature 60.0 - 120 °C
Average value: 3.93 % Grade Count:1
Elongation at Yield 2.00 - 2.00 %
@Temperature 90.0 - 120 °C
Average value: 2.00 % Grade Count:1
Modulus of Elasticity 1.93 - 8.40 GPaAverage value: 4.37 GPa Grade Count:13
 2.40 - 3.40 GPa
@Temperature 60.0 - 120 °C
Average value: 2.87 GPa Grade Count:1
Flexural Yield Strength 75.8 - 235 MPaAverage value: 125 MPa Grade Count:20
Flexural Modulus 0.981 - 9.51 GPaAverage value: 3.77 GPa Grade Count:23
Izod Impact, Notched 0.588 - 1.60 J/cmAverage value: 0.986 J/cm Grade Count:19
 0.5339 - 1.0678 J/cm
@Temperature -40.0 - -30.0 °C
Average value: 0.774 J/cm Grade Count:4
Izod Impact, Unnotched 5.34 - 16.0 J/cmAverage value: 8.01 J/cm Grade Count:4
Charpy Impact Unnotched 1.00 - 6.50 J/cm²Average value: 3.50 J/cm² Grade Count:6
 5.00 - 5.00 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 5.00 J/cm² Grade Count:1
Charpy Impact, Notched 0.350 - 1.40 J/cm²Average value: 0.788 J/cm² Grade Count:10
 0.400 - 0.400 J/cm²
@Temperature -30.0 - -30.0 °C
Average value: 0.400 J/cm² Grade Count:1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 52.0 - 3.00e+16 ohm-cmAverage value: 1.23e+16 ohm-cm Grade Count:12
Surface Resistance 39.0 - 6.00e+15 ohmAverage value: 1.28e+15 ohm Grade Count:9
Dielectric Strength 20.0 - 49.0 kV/mmAverage value: 31.3 kV/mm Grade Count:3
Comparative Tracking Index 175 - 250 VAverage value: 203 V Grade Count:8
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 - 50.0 µm/m-°CAverage value: 45.9 µm/m-°C Grade Count:8
CTE, linear, Transverse to Flow 50.0 - 75.0 µm/m-°CAverage value: 63.8 µm/m-°C Grade Count:6
Maximum Service Temperature, Air 110 - 160 °CAverage value: 147 °C Grade Count:6
Deflection Temperature at 0.46 MPa (66 psi) 126 - 250 °CAverage value: 153 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 95.0 - 207 °CAverage value: 140 °C Grade Count:23
Vicat Softening Point 130 - 239 °CAverage value: 159 °C Grade Count:11
Minimum Service Temperature, Air -40.0 °CAverage value: -40.0 °C Grade Count:4
Flammability, UL94 HB - 5VAGrade Count:17
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 265 - 310 °CAverage value: 289 °C Grade Count:4
Melt Temperature 249 - 320 °CAverage value: 287 °C Grade Count:16
Mold Temperature 60.0 - 120 °CAverage value: 89.2 °C Grade Count:18
Drying Temperature 80.0 - 110 °CAverage value: 98.3 °C Grade Count:16
Moisture Content 0.0200 - 0.100 %Average value: 0.0600 % Grade Count:4
Injection Pressure 68.9 - 103 MPaAverage value: 86.2 MPa Grade Count:3
Vent Depth 0.00254 - 0.00381 cmAverage value: 0.00349 cm Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Overview of materials for Polyphenylene Ether, Impact Grade
Overview of materials for Polysulfone (PSU)
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
Overview of materials for Polycarbonate, Molded

O4411 / 78323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.