MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Syncure™ S1016A Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System.

Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1016A / 5 phr S1000B system; and cured for 6 hours in water at 90 degree C. Modulus measured on a 95 phr S1016A / 5 phr S1037B system. Pellet appearance is 1/8 cylindrical.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.530 g/ccGeon® 1169; Internal Method
 0.949 g/ccASTM D1505
Melt Flow 0.46 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A; ASTM D1238
Deformation 2.0 %
@Temperature 131 °C,
Time 3600 sec
500 g; UL 1581
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 31.0 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 30 %SYV-40; Hot Creep Elongation
 400 %Type IV, 510 mm/min; ASTM D638
Flexural Modulus 9.65 MPaASTM D790
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
FormsPellets
Gel Content80%ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Regional AvailabilityNorth America
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LS4201R Polyethylene Insulation Compound, Crosslinkable
Syensqo (Solvay Specialty Polymers) Polidan® EC/51 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® S/I 20 Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® T/A Polyethylene, Crosslinked (XLPE)
Syensqo (Solvay Specialty Polymers) Polidan® T/A-LX Polyethylene, Crosslinked (XLPE)

PH0POL0327 / 144896

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.