MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A 218G2 V30 Black 34N Nylon 66, 30% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Product Description: Ultramid® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This grade has been specially designed to improve its resistance to automotive cooling liquids, increasing lifetime of parts in permanent contact with such liquids.

Availability: Africa & Middle East; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer; Hydrolysis Resistant

Features: Good Flow; Good Mold Release; Heat Stabilized – Inorganic; High Glycol Resistance; Hydrolysis Resistant

Use: Automotive Applications; Pump Parts

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Appearance: Black

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.36 g/cc0.0491 lb/in³ISO 1183
Water Absorption 0.80 %
@Time 86400 sec
0.80 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.011 cm/cm0.011 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 195 MPa28300 psiISO 527-2
Elongation at Break 3.0 %3.0 %ISO 527-2
Tensile Modulus 10.0 GPa1450 ksiISO 527-1
Flexural Strength 290 MPa42100 psiISO 178
Flexural Modulus 9.17 GPa1330 ksiISO 178
Izod Impact, Notched (ISO) 10.1 kJ/m²4.80 ft-lb/in²ISO 180/A
Charpy Impact Unnotched 8.61 J/cm²41.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.09 J/cm²5.20 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
IEC 60695-11-10,-20
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 280 °C518 - 536 °F
Middle Barrel Temperature 275 - 285 °C527 - 545 °F
Front Barrel Temperature 280 - 290 °C536 - 554 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2084 / 310777

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.