MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

TBA ECP 526 Extra' Conductive Waterbased anti slip epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: ECP 526 'Extra' is a high quality water borne two pack epoxy system. Environmentally friendly, it offers the advantages of low odour, and easy cleaning of equipment with water and anti-slip properties. Additionally the coating has an advantage over conventional anti-slip coatings as it can be applied by virtually any method, including spraying. It is very aesthetically appealing as it is made without the traditional additives used in anti-slip coatings such as grit and metal shards and provides a silky matte finish. ECP 526 'Extra' finds application in areas such as floor coatings (particularly where the previous coating is unknown as solvent will attack many coatings causing them to lift).
Typical installations include:
  • Electrical industry.
  • Petrol/ Chemical industries.
  • Water treatment plants.
  • Hospitals.
  • Food Industry- Machinery and surfaces.
  • And many other industrial uses
ECP 526 'Extra' exhibits excellent mechanical properties which will withstand abrasion and impact, as well as giving good resistance to a wide range of chemicals including: Oils, Fats, Solvents, Acids and Alkalis. The electrical properties of the paint are permanent and independent of humidity; additionally a conductive underlay is not required for grounding the system. Additionally ECP 526 'Extra' provides the option of directly grounding racking/shelving used for storing ESSD’S (electro static sensitive devices) to the floor. For personnel grounding applications the product is best used in conjunction with suitable electrostatic dissipative (anti static) footwear, e.g. ECP 1450 series foot straps.

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.37 g/cc1.37 g/cc
Solids Content 58 %58 %
pH 8.58.5
Viscosity 250 cP250 cPICI cone and plate
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 1.00e+6 ohm<= 1.00e+6 ohm2 coats
 
Thermal PropertiesMetricEnglishComments
Flash Point 163 °C325 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 60.0 min60.0 min
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorLight Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTBA022 / 281500

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.