MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Magnesium WE54A-T6, Sand/Permanent Mold Castings
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: Commercial and sand castings used in the solution heat treated and artificially aged (T6 temper) condition. Castings retain properties at high temperatures (300°C) for short term applications (up to 1000 hr) and are pressure tight and weldable.

Key Words: UNS M18410; Mg; AMS 4426; ASTM B 80; European EN 1753 MC 95310
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 75 - 95500 kg load, 10 mm ball
Tensile Strength, Ultimate 36000 psi
Tensile Strength, Yield 24000 psi
Elongation at Break 2.0 %in 50 mm
Tensile Modulus 44.4 GPa
Compressive Yield Strength 25000 psi
Compressive Strength 59.5 ksi
Poissons Ratio 0.27
Shear Modulus 17.5 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000173 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 370 J/gEstimated from trends in similar Mg alloys.
CTE, linear 26.0 µm/m-°C
@Temperature 0.000 - 100 °C
Estimated from similar Mg alloys.
 27.0 µm/m-°C
@Temperature 20.0 - 200 °C
Estimated from similar Mg alloys
Specific Heat Capacity 1.00 J/g-°CTypical Mg alloy value.
Thermal Conductivity 52.0 W/m-K
Melting Point 550 - 640 °C
Solidus 550 °C
Liquidus 640 °C
 
Processing PropertiesOriginal ValueComments
Casting Temperature 750 - 820 °CSand Casting
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu <= 0.030 %
Magnesium, Mg 91.1 %As Remainder
Manganese, Mn <= 0.15 %
Nickel, Ni <= 0.0050 %
Other, each <= 0.20 %
Other, total <= 0.30 %
Rare Earths 3.0 %
Silicon, Si <= 0.010 %
Yttrium, Y 4.75 - 5.5 %
Zinc, Zn <= 0.20 %
Zirconium, Zr 0.40 - 1.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
420 Stainless Steel
Magnesium WE43-T6, Cast
Magnesium ZC71-T6
Magnesium AM60B-F, Die Cast
Magnesium AM60A-F, Die Cast

MMWE55 / 12465

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.