MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3847MR Polypropylene, Radiation Resistant - Clarified - High Flow for Injection Molding
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: TOTAL Petrochemicals Polypropylene 3847MR offers good processability, excellent clarity, good toughness and good resistance to typical levels of gamma radiation used to sterilize polypropylene.Easy Flow TOTAL Polypropylene 3847MR exhibits exceptionally easy flow characteristics.

Recommended Applications. TOTAL Polypropylene 3847MR is recommended for injection molding laboratory and medical applications; however, due to its unique combination of properties, other applications may exist.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D1505
Melt Flow 45 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 32.0 MPaASTM D638
Elongation at Yield 9.0 %ASTM D638
Flexural Modulus 1170 MPaASTM D790
Izod Impact, Notched 30.0 J/mASTM D256A
Izod Impact, Unnotched NBASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 157 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Flint Hills P9M7R-056 Specialty Homopolymer Polypropylene
Flint Hills P5M6K-080 Polypropylene Random Copolymer
LyondellBasell Pro-fax PF531 Polypropylene Homopolymer, Radiation Resistant
Dow HDPE 04452N High Density Polyethylene

PTOTAL819 / 130544

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.