MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polyplastics Duracon® WW-09 CF2001 Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Easy Sliding. High viscosity.

Information provided by Polyplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.029 cm/cm
@Thickness 2.00 mm
0.029 in/in
@Thickness 0.0787 in
Cavity pressure 60 MPa; 60x60x2; ISO 294-4
Linear Mold Shrinkage, Transverse 0.023 cm/cm
@Thickness 2.00 mm
0.023 in/in
@Thickness 0.0787 in
Cavity pressure 60 Mpa; 60x60x2; ISO 294-4
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575ISO 2039-2
Tensile Strength 58.0 MPa8410 psiISO 527-1,2
Elongation at Break 40 %40 %Nominal; ISO 527-1,2
Tensile Modulus 2.60 GPa377 ksiISO 527-1,2
Flexural Strength 75.0 MPa10900 psiISO 178
Flexural Modulus 2.20 GPa319 ksiISO 178
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
Coefficient of Friction, Dynamic  0.14
@Pressure 0.980 MPa
0.14
@Pressure 142 psi
Thrust, vs C-Steel. 30 cm/s; JIS K7218
 0.16
@Pressure 0.490 MPa
0.16
@Pressure 71.1 psi
Thrust, vs C-Steel. 30 cm/s; JIS K7218
 0.34
@Pressure 0.0600 MPa
0.34
@Pressure 8.70 psi
Thrust, vs M90-44. 15 cm/s; JIS K7218
K (wear) Factor  <= 1.00 x 10-8 mm³/N-M
@Pressure 0.490 MPa
<= 0.496 x 10-10 in³-min/ft-lb-hr
@Pressure 71.1 psi
Thrust, vs C-Steel, steel side. 30 cm/s; JIS K7218
 <= 1.00 x 10-8 mm³/N-M
@Pressure 0.980 MPa
<= 0.496 x 10-10 in³-min/ft-lb-hr
@Pressure 142 psi
Thrust, vs C-Steel, steel side. 30 cm/s; JIS K7218
 26.0 x 10-8 mm³/N-M
@Pressure 0.980 MPa
12.9 x 10-10 in³-min/ft-lb-hr
@Pressure 142 psi
Thrust, vs C-Steel, material side. 30 cm/s; JIS K7218
 42.0 x 10-8 mm³/N-M
@Pressure 0.490 MPa
20.8 x 10-10 in³-min/ft-lb-hr
@Pressure 71.1 psi
Thrust, vs C-Steel, material side. 30 cm/s; JIS K7218
 900 x 10-8 mm³/N-M
@Pressure 0.0600 MPa
447 x 10-10 in³-min/ft-lb-hr
@Pressure 8.70 psi
Thrust, vs M90-44, material side. 15 cm/s; JIS K7218
 7820 x 10-8 mm³/N-M
@Pressure 0.0600 MPa
3880 x 10-10 in³-min/ft-lb-hr
@Pressure 8.70 psi
Thrust, vs M90-44, M90-44 side. 15 cm/s; JIS K7218
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+14 ohm-cm6.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Strength 19.0 kV/mm
@Thickness 3.00 mm
483 kV/in
@Thickness 0.118 in
IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C181 °FISO 75-1,2
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLPL9876 / 305549

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.