MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Epoxy Technology EPO-TEK® H75 Thermally Conductive, Electrically Insulating Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Material Description: A two component, high Tg, thermally conductive, electrically insulating epoxy designed for semiconductor packaging including heat sinking, hermetic sealing, and opto-electronic assemblies. It may be considered a higher viscosity alternative to EPO-TEK® H74.

Information Provided by Epoxy Technology

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/ccPart B
 2.27 g/cc2.27 g/ccPart A
Particle Size <= 50 µm<= 50 µm
Viscosity 300000 - 400000 cP
@Temperature 23.0 °C
300000 - 400000 cP
@Temperature 73.4 °F
0.5 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9595
Tensile Modulus 6.52 GPa946 ksiStorage
Shear Strength 13.04 MPa1892 psiLap
 >= 46.9 MPa>= 6800 psiDie
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 2.00e+12 ohm-cm>= 2.00e+12 ohm-cm
Dielectric Constant 5.37
@Frequency 1000 Hz
5.37
@Frequency 1000 Hz
Dissipation Factor 0.0080
@Frequency 1000 Hz
0.0080
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 29.0 µm/m-°C16.1 µin/in-°FBelow Tg
 90.0 µm/m-°C50.0 µin/in-°FAbove Tg
Thermal Conductivity 0.660 W/m-K4.58 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C482 °FContinuous
 350 °C662 °FIntermittent
Minimum Service Temperature, Air -55.0 °C-67.0 °FContinuous
 -55.0 °C-67.0 °FIntermittent
Glass Transition Temp, Tg >= 100 °C>= 212 °FDynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min
Decomposition Temperature 416 °C781 °FDegradation Temperature
 
Processing PropertiesMetricEnglishComments
Cure Time  5.00 min
@Temperature 150 °C
0.0833 hour
@Temperature 302 °F
Minimum
 30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
Minimum
Pot Life 180 min180 min
Shelf Life 12.0 Month
@Temperature 25.0 °C
12.0 Month
@Temperature 77.0 °F
 
Descriptive Properties
ColorAmberPart B
 GrayPart A
ConsistencyThick paste
Mix Ratio by Weight100:3.3
Number of ComponentsTwo
Weight Loss<0.05%200°C
 0.2%300°C
 0.8%250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Epoxy Technology EPO-TEK® H61LV Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H61 Thermally Conductive Epoxy
Epoxy Technology EPO-TEK® H63 Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H61ND Thermally Conductive, Electrically Insulating Epoxy
Epoxy Technology EPO-TEK® H73 Thermally Conductive, Electrically Insulating Epoxy

PPOXYT083 / 141122

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.